Dear Mr Anand,

Your welding current may not exceed 200 to 220 amps continuous range.

Regards,

Nimesh Chinoy
SigmaWeld
www.electronicsdevices.com

Sent on my BlackBerry® from Vodafone


From: Pushpraj Anand <pushprajanand34@gmail.com>
Sender: materials-welding@googlegroups.com
Date: Wed, 12 Jan 2011 13:30:14 +0530
To: <materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: [MW:9188] Regarding GTAW Welding Machine

Dear All,
 
 
We are going to weld 4 mm / 6 mm stainless steel plate.Filler wire dia is 2.4 mm and tungsten electrode dia is 1.6 mm.
 
for welding machine what should be the output current range and maximum continuous current at 100% duty cycle. please suggest me which welding machine is best for this application .
 
we are manufacturing this product in india.

--
Regards,
Pushpraj Anand

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...