Tuesday, January 11, 2011

Re: [MW:9172] EN 287-1 WPQT Range Issue

Hi,
Yes.Your interpretaion is correct.

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Sat, 1/8/11, limesh M <limesh78@gmail.com> wrote:

From: limesh M <limesh78@gmail.com>
Subject: [MW:9151] EN 287-1 WPQT Range Issue
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Saturday, January 8, 2011, 8:23 PM

 Dear All,
 

Welder qualification Code: EN 287-1, 2004 Edition.

Product type used for welder qualification: Plate
Welding position:PA
 
I have qualified a welder on 'PA' position in plate material. As per EN287-1 table 7, the welder is qualified to weld PA, PB positions  and not qualified to weld any other positions.But foot note 'a' says, additionally the requirements of 5.3 and 5.4 shall be observed.So,I need clarification on the following queries as the clauses confusing me.
 1. Is the welder qualified to weld pipe based on above qualification, if pipe diameter is, D≥150mm (PA, PB, PC) positions?

 

2. Is the welder qualified to weld pipe based on above qualification, if pipe diameter is, D≥500mm for all welding positions?
 
 
Regards,
Limesh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...