Re: [MW:9162] Impact test temperature required............

Dear Govi,

(1)- Since the dsign MDMT is -20 c, Impact test shall be done at same temperature or below that regardless ASME B31.3 recommendations.

(2)- For mechanical testing requirements, please check API 5l spec and Client spec.

Regards
Manpreet Singh


On Sun, 09 Jan 2011 09:54:54 +0530 Govindarajan Shanmugam wrote
>
Dear All,
 

I have a mill test certificate (MTC) for API 5L X60-PSL2- 30inch dia by 17.5mm thk-SAW welded pipe-. Technical delivery condition is mentioned as TM in the MTC. Samples for mechanical testing has undergone SR. MTC shows that impact testing for the plate material was done at minus 10 deg C.

As per the Client spec, impact testing is to be done in acc with ASME B31.3 Para 323.3.

Project piping specification shows Pressure/Temp limits of 50barg/ -20 to 43 deg C.

 

Please clarify

  1. whether impact test done at minus 10 deg C is correct or it should have been done at minus 20 deg C.
  2. Whether any mechanical testing is required on the long seam weld of the SAW welded pipe.
with regards
Govi.

>

--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...