If the joint size is 48” and repair is on 200mm only, still we need to cutout the joint or remove the entire weld for that portion ( 200 -300 mm) and re-weld. 

 

 

With Kind regards,

 

S.Elumalai.


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Shanmugam Palanisamy
Sent: Sunday, January 09, 2011 12:28 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:9154] Weld Repair

 

Dear Taufiq,

 

Doing welding many time at the same location, the base matel mechnical properity well get change. To avoid the properity change, better to cut and reweld.

 

regards

 

Samy

On Sat, Jan 8, 2011 at 4:34 AM, Taufiq <taufiq_civ@yahoo.com> wrote:

Dear all,

Our client specification clearly stated that filler and cap weld may
be repaired a maximum of 2 times using qualified procedure. I will
appreciate if anyone can tell me what is going on if we repair the
weld for more than 3 times?

Thank you and regards,

taufiq

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...