Dear experts,

Please advise the hardness value of SA516 for all grade (with ref. detail) since it is not mentioned either in ASME sect. II/IX or the correspond ASTM.

Even we can take the figure from conversion table or theoretical formula, I'm not confidence of using this as reference.

Appreciate for your feedback on this

Thanks and Rgds
A.D. Wenda - Indonesia

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...