Thursday, January 20, 2011

[MW:9346] RE: 9343] THICKNESS LOSS IN UNSO6625

Dear Sir:

Please see referenced documents(Clause 2) in ASTM B564,I think these referenced STDs may be useful.

 

Regards

Bazrafshan

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ali Asghari
Sent: Thursday, January 20, 2011 9:16 AM
To: materials-welding@googlegroups.com
Subject: [MW:9343] THICKNESS LOSS IN UNSO6625

 

Dear All

in some cases in UNS06625 fittings, alittle thickness reduced by grinding, now in which section of ASTM  i find the acceptance criteria of thickness loss?(i don't find in ASTM B564)

REGARDS

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...