Dear all,
 
I have a material A350 LF2, CL1  with UTS of 724MPa (As mentioned in TC of Manufacturer).
 
As per ASME Sec IIA, requirement is 485 - 655 Mpa.
 
The higher value of UTS beyond the spec requirements is aceptable?
 
Thanks.
Regards,
JJ

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.