Dear All,
Presently we have conducted a Destructive test-(All Weld Tensile Test) for a E6010 and E7010 electrode,in which the Elongation Value is 20.2 %and 20%, whereas the required value as per the specification is 22%.Kindly please tell me if this can be acceptable or any consideration can be given to this test value ?
Also kindly please tell me for carrying out Charpy V Impact Test for 10mm X 5mm X15 mm ,Specimen for X65 Grade material Pipe welded with E6010 and E7010-P1 what is the temperature it has to be tested.?
Kindly give your suggestions at your earliest..
Regards,
Eldho Isaac,
Inspection Engineer.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments