Wednesday, January 12, 2011

[MW:9197] R: 9195] corrosion on grith of weld joint

I don’t know which code you follow but if is ASME you can to try tell that the thickness may be reduced until 12,5% reference code ASME B 36.10 for carbon steel pipes and  ASME B 36.19 for stainless steel pipes

bye

 

Claudio

 

 

Da: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Per conto di sujay kumar
Inviato: mercoledì 12 gennaio 2011 12:41
A: materials-welding@googlegroups.com
Oggetto: [MW:9195] corrosion on grith of weld joint

 

Dear All,

 

we facing a problem of corrosion on pipe adj cent to the butt weld joint, this happened due to unpainted of that area. as per project specification for weld girth be should be exposed (uncovered and unpainted)  and temporary covered with making tape and to be removed during  test. rest of pipe was painted,

 

 this  was found during blasting time,after hydro test.

 

can anybody say how to repair or rectify that area with reference to code (newly constructed line).

 

your reply is highly appreciable.

 

Regards

 

Sujay

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...