Dear Krishna,
P-NO ,1, And material is is 2062 , so you done
the root with E7018 OF 2.4mm, Welding Electrode and final caping with
also same , but you have choice to done the final caping with 3.5mm
welding rod, no need of E9018

On Jan 5, 4:46 pm, "manpreet " <manpreetsi...@rediffmail.com> wrote:
> Dear Krishna,Please explain your query in detail,if you are qualifying PQR then you can always choose different filler metals for different passes or&nbsp;If you&nbsp;have WPS which mention different filler metal for Cap, Also the title is vague&nbsp;"WPS and PQR for P 1 material and P 5", Please clarify.RegardsManpreet SinghOn Wed, 05 Jan 2011 16:59:32 +0530 Saamy wrote&gt;Dear All !&gt; Could you help me any one... We have IS 2062 material&gt;for rail welding... the manufacturer recommend for E 7018 for root,&gt;hot and filling and E9018 for capping on IS 2062... My Question is how&gt;to allow E 9018 on IS 2062? Both electrodes have different A No...&gt;That is essential variable... So please give advice...&gt;&gt;-- &gt;To post to this group, send email to materials-welding@googlegroups.com&gt;To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com&gt;For more options, visit this group's bolg athttp://materials-welding.blogspot.com/>Theviews expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.&gt;

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...