Dear ,
 
At, what temp you want to do impact test,it may be -29 c or -40 c. first of all keep the specimen at required temp then proceed for the test,keep the test piece on machine set for chappy scale.
 
temperature is desire by job base or specified.
 
thanks and regards
Sujay

On Sun, Oct 24, 2010 at 10:12 AM, mechsen <senbe381@gmail.com> wrote:
DEARS,
    HOW  WE CONFIRM CHARPY V-NOTCH IMPACT TOUGHNESS TEST DONE  ON
LOW TEMPERATURE SATISFIED ? I  WANT TO KNOW TEMPERATURES.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...