Friday, October 22, 2010

Re: [MW:7699] Chemical properties of SA 213 Gr. 304H

never chem. will change in the process of HT.
 

175, R.Kesavamoorthi,

Principal surveyor,

Quest (pvt.) Ltd.,

Ranipet.




From: agstes <agstes@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thu, 21 October, 2010 1:09:15 PM
Subject: [MW:7673] Chemical properties of SA 213 Gr. 304H

Dear All,
 
Is there any change in chemical properties prior to solution annealing and after solution annealing of SA 213 Gr. 304H ( solution annealing temp 1040 degree centigrade) e.g. % of carbon specifically.
 
Thanks well in advance.
 
Regards,
 
Shinde

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...