Friday, October 22, 2010

RE: [MW:7698] Query regarding welding of material ASTM A 106 grade B To ASME B 36.10

Hi,
Yes . you can use since the metals are same S.No. and according to QW424 your wps can use for both.
 
Thanks & Regards,
 
(karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Thu, 10/21/10, B.Raghuram <raghurambathula@gmail.com> wrote:

From: B.Raghuram <raghurambathula@gmail.com>
Subject: RE: [MW:7680] Query regarding welding of material ASTM A 106 grade B To ASME B 36.10
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: Thursday, October 21, 2010, 7:03 PM

What is your construction code? B31.3 require new qualification.

Sent from my Nokia phone
-----Original Message-----
From: sumit jaura
Sent:  21/10/2010 11:10:47 am
Subject:  [MW:7671] Query regarding welding of material ASTM A 106 grade B To ASME B 36.10

Dear All,

We have qualified WPS for the welding of material ASTM A 106 grade B To ASME
B 36.10. " Using the same WPS can we go for the welding of material A694 F65
To API 5L X65 and " API 5L X65 To A105 Grade B "

Please clearify in deatails.

Thanks in advance.

Matter is Urgent.

Thanks & Rgards,

Sumit Jaura
worleyParsons India
Mob : +91 9541454764

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...