Re: [MW:7610] Welding of A312 Gr.TP321H

no need to requalify
vanchi

On Sun, Oct 17, 2010 at 12:43 PM, ARUN KUMAR <arunku72@hotmail.com> wrote:
Dear All,
 
I need your valuable advice on following.
 
I need to carry out the welding of A312 Gr. TP321 H ( GTAW process) with a WPS qualified for P8- P8 material. In the WPS it is mentioned that to use ER 347 H for welding A312 Gr.TP321 H.
 
In ASME, section II, there is no F no classification for ER 347 H ( other filler ER308 H & ER316 H are classified in 5.9)
 
The filler wire is supplied by ESAB and theire Material cert is showing only ER 347 ( SFA 5.9) with carbon % .04 ( As per section II ,Carbon % for ER 347 is max .08%)
 
Since there is difference in C %, do I need to requalify the WPS using  the above filler ( ER 347 with C % .04)?
 
Thanks and regards,
 
Arun

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...