As per code section 1 , under repair of defects, PW 40.3.4.d, pl refer for SMAW ( 4xcore dia),also given in code section 8,                                     for GTAW general engineering practice-width shall not be more than 10mm
 
kgp
 
 
On Sat, Oct 16, 2010 at 6:32 PM, limesh M <limesh78@gmail.com> wrote:
Dear All,
 
I heard about weaving ,which is applicable in SMAW.If I am crossing the weaving barrier as per manufacturer recommendation,ie,  2.5 X dia of electrode or 3 X dia of electrode what would happen?
 
Is weaving applicable in GTAW? If applicable what would be the weaving range?
 
 
 
Regards,
 
Limesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...