Hi, For WPS fluid ets.,are all no need. You can use your old WPS.But you check with the old WPS range and qualifications to your current project.If it suits..then go ahead. Karthikeyan.S QA/QC Manager Getabec Energy Co.,Ltd. 379,Moo6,Soi8,Nikhomphatana, Rayong-21180, Thailand. Phone: 0066 38 897035-8 (Off) Fax: 0066 38 897034 Hand Phone: 0066 892512282
--- On Mon, 10/4/10, Eduardo Calva <eduardocalva@hotmail.com> wrote: From: Eduardo Calva <eduardocalva@hotmail.com> Subject: [MW:7346] Welding procedure qualification for Hot tap To: materials-welding@googlegroups.com Date: Monday, October 4, 2010, 2:29 PM
Can anybody tell me which are the variables to take in account in order to qualify a WPS for hot tap?, I mean, is it just diameter, thickness, material spec., ?, or do I have to take account temperature, flow, fliud characteristics? Another question is: Can I use a old WPS for HT used in other projects? Eduardo Calva -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
|
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment