Monday, October 4, 2010

Re: [MW:7337] RE: 7319] Test piece from pipe...

Dear Mr. Girish,
 
You can refer 463.1(f) NOTCH TOUGHNESS TEST SPECIMEN WELD LOCATION if the specimen is qualified in 5G or 6G.
 
arvinda.

On Sun, Oct 3, 2010 at 7:05 PM, Harish Kannepalli <harishkannepalli@gmail.com> wrote:
Dear Girish,
                   As per ASME you have to take CVN from Weld center line, HAZ. Refer ASME Sec 8 Div2 for CVN requirements. There u have the locations, energy requirements,etc.

2010/10/3 Shadab Alam Ansari <shadabansarialam@gmail.com>

Dear Girish,

In which position the welding was done?

 

Regards

Shadab Alam Ansari

Welding Engineer

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of giraish real
Sent: Saturday, October 02, 2010 4:54 PM
To: materials-welding@googlegroups.com
Subject: [MW:7319] Test piece from pipe...

 


Dear all

 

I want to Qualify a PQR in pipe  Material LTCS-A333Gr6.Pipe Dia is 8".

 

now my Question is for Destructive test (IMPACT) ,from which location I have to cut?

 

please give ASME reference also.


Girish K. Vora

09978910870

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
regards,
Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...