                   As per ASME you have to take CVN from Weld center line, HAZ. Refer ASME Sec 8 Div2 for CVN requirements. There u have the locations, energy requirements,etc.

2010/10/3 Shadab Alam Ansari <shadabansarialam@gmail.com>

Dear Girish,

In which position the welding was done?

 

Regards

Shadab Alam Ansari

Welding Engineer

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of giraish real
Sent: Saturday, October 02, 2010 4:54 PM
To: materials-welding@googlegroups.com
Subject: [MW:7319] Test piece from pipe...

 


Dear all

 

I want to Qualify a PQR in pipe  Material LTCS-A333Gr6.Pipe Dia is 8".

 

now my Question is for Destructive test (IMPACT) ,from which location I have to cut?

 

please give ASME reference also.


Girish K. Vora

09978910870

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
regards,
Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...