Sunday, October 3, 2010

[MW:7335] Re: NACE-Corrosion Coures

http://www.naceindia.org/CIP%20Brochure.pdf
you may down load brochure from the above link, including
registration form

On Oct 3, 9:15 pm, Dinesh Kumar <rdinesh.tri...@yahoo.com> wrote:
> Dear Sir,
>
> Please tell me in india,institutes conducting "NACE-Corrosion Courses & Exam"
>
> Regards/Dinesh Kumar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...