Sunday, October 3, 2010

[MW:7330] jig diamention for bend test as per AWS D1.1

what is the diamention of jig used for side bend test as per aws d1.1,material is api 5Lx52,?


--- On Sat, 2/10/10, Manuel Haces Valdez <manuelhacesvaldez@gmail.com> wrote:

From: Manuel Haces Valdez <manuelhacesvaldez@gmail.com>
Subject: Re: [MW:7322] Electrode for cast steel
To: materials-welding@googlegroups.com
Date: Saturday, 2 October, 2010, 10:24 PM

There are several electrodes for this, they are based in Nickel, so even you can use a Stainless electrode. Regards.

2010/9/30 Larry <quality@unieng.com.au>

Hi,

 

Can anybody suggest a good electrode for cast steel?

 

No code applies, just common welding.

 

 

Thanks in advance.

 

 

 

Cheers,

Larry

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...