Monday, September 27, 2010

Re: Re: [MW:7216] problem SS 316 flange to pipe welding


Hi,

whenever welding plate flange with pipe you have to give clearance of
1.5 mm on flange . same OD same ID how it will go? even drive fit it
require some clearance . this is the reason the job spoiled. while
welding steel will expand u have to consider coefficient of expansion
steel too.

for good sound welding insert the pipe smoothly inside the flange and
keep 6 mm below the face of flange face and weld fillet welding and
pipe OD to Flange ID weld fillet of 8 mm. .


Muthu Barathi P

Sr Manager QA/QC
AFCONS
On Mon, 27 Sep 2010 11:17:41 +0530 wrote
>please provide the sketch showing arrangement during welding. Also
indicate the area where the dimensions are going out. So that people
from the group can understand your problem and answer


On 24 September 2010 19:45, rmsengineering
wrote:

We are fabricating flanged connections for one of our customers

 flange dia 350  id220 and thickness is28 mm  is   joined to 220od

8thk pipe     After welding it is observed that out of 6 jobs in 4

jobs the flange has warped in two jobs it is beyond repairs to such a

extent that the face & od to be machined is beyond tolerances (od run

out is 10 mm face is out by 7 mm )

Anticipating this problem we have press  fit the components and made

the arrangements for rapid cooling but still this has happened

Now we need to manufacture 10 more flanged connection of the same

type

what precautions should be taken

The welding is done by GTAW 5mm thk fillet all over 5%thoriated 3mm

rod with filler ss 316L 2,5thk current 180Amps inside welding was

fused where as for out side welding filler was given



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding-
unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-
welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.



--
C. K. Purohit
Eng-Tech Weld1
Sr Welding Inspector






--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-
unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>


Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

P Muthu Barathi
Mobile No:09967300544

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...