Re: [MW:7279] difference between E7018 and E7018-1

Hi,
 
E7018 is impact tested @ -30 Deg C
E7018-1 is impact teted @ -46 Deg C.,
 
I think '-1' is not having anyspecific meaning as per code like 70=70000 psi etc.
 
Cheers!
 
Rajasekhar.

On Wed, Sep 29, 2010 at 3:51 PM, Adi <adinraos@gmail.com> wrote:
Hi everybody

What is difference between E7018 and E7018-1
what is meant by "-1"

Adi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...