Wednesday, September 29, 2010

Re: [MW:7278] Using WPS qualified as per D1.1 to weld pipework as perASME IX

Hi,
 
What about the mechanical test coupon sizes for tensile and bend tests, AWS is having different requirements for mechanical test coupon size and allowances than ASME Sec-IX.
I think we can not club these two codes together, please correct me if i am wrong.
 
Cheers!
 
Rajasekhar.
On Tue, Sep 28, 2010 at 10:53 PM, John Henning <jhenning@deltak.com> wrote:

Phillip,

 

If you qualified a PQR to AWS D1.1 you most likely can use the data to write a PQR to ASME Section IX.  You will have to review the data taken during the PQR test and mechanical test results to assure that all the requirements of Sc IX are met.  If your data and test results are sufficient then you may write a new PQR in an acceptable Sc IX format.  With the PQR you will write the WPS with limitations based on the ASME PQR and Sc IX permitted ranges. 

 

Think about it, if the data exists and properly qualifies what you will do in practice, what practical reason would there be to perform another PQR test.  You would simply repeat the same test, with the same basic parameters, process, base metals, weld consumables and, theoretically, have the same results.  The reason to perform the PQR in the first place is to verify that a sound weld with appropriate room temperature mechanical properties can be obtained when welded under certain conditions.

 

 As long as the data and results meet the requirements, it can be applied to any Code.  Thus if I perform a weld under EN rules with observation of a Notified Body Inspector, I can write from that data a PQR and WPS to EN 15614, ASME  Sc IX, and/or AWS if I have made the effort to assure that the data and test results satisfied the qualification requirements for all three.  The WPS ranges of qualification will most likely be different but that doesn't affect the quality of the input data.

 

{Note the obvious -  that an AWS prequalified welding procedure may not be warped into a Sc IX welding procedure as there is no PQR}

 

John

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Endri Prasetyo
Sent: Tuesday, September 28, 2010 11:20 AM

Subject: Re: [MW:7257] Using WPS qualified as per D1.1 to weld pipework as perASME IX

 

Dear Philip,

In my opinion cannot. Your procedure is only for D1.1 application.
When we will apply another code, so we have to follow the code we will refer to.

Kind Regards,
Endri

Sent from my BlackBerry®


From: "Philip, Taiye (Lagos)" <Taiye.Philip@deltaafrik.com>

Date: Tue, 28 Sep 2010 13:00:41 +0100

Subject: [MW:7250] Using WPS qualified as per D1.1 to weld pipework as per ASME IX

 

Hello gents,

 I have a WPS qualified as per D1.1 8 inches for welding structural work, in 6G position,

My query is can I use these procedure to weld pipe work as per ASME IX for the same material?

Pls I need further clarification with codes support.

 

Regards

Philip Taiye

 

 


*** WORLEYPARSONS GROUP NOTICE *** "This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it. If you have received this email in error, please notify us immediately by return email and delete the email and any attachments. Any personal views or opinions expressed by the writer may not necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...