Wednesday, September 29, 2010

Re: [MW:7259] Using WPS qualified as per D1.1 to weld pipework as perASME IX

Hi,

Please find below the extraction of ASME Sec.IX.Please go thru tjis and also refer Article-V of Section-IX.

 

Thanks & Regards,

 

(Karthik)

 

QW-100.1 A Welding Procedure Specification (WPS)

is a written document that provides direction to the welder

or welding operator for making production welds in accordance

with Code requirements. Any WPSs used by a manufacturer

or contractor that will have responsible operational

control of production welding shall be a WPS that has

been qualified by that manufacturer or contractor in accordance

with Article II, or it shall be an AWS Standard

Welding Procedure Specification (SWPS) listed in Appendix

E and adopted by that manufacturer or contractor in

accordance with Article V.


Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Tue, 9/28/10, Endri Prasetyo <endri.prasetyo@gmail.com> wrote:

From: Endri Prasetyo <endri.prasetyo@gmail.com>
Subject: Re: [MW:7257] Using WPS qualified as per D1.1 to weld pipework as perASME IX
To: materials-welding@googlegroups.com
Date: Tuesday, September 28, 2010, 11:20 PM

Dear Philip,

In my opinion cannot. Your procedure is only for D1.1 application.
When we will apply another code, so we have to follow the code we will refer to.

Kind Regards,
Endri

Sent from my BlackBerry®

From: "Philip, Taiye (Lagos)" <Taiye.Philip@deltaafrik.com>
Sender: materials-welding@googlegroups.com
Date: Tue, 28 Sep 2010 13:00:41 +0100
To: <materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: [MW:7250] Using WPS qualified as per D1.1 to weld pipework as per ASME IX

Hello gents,

 I have a WPS qualified as per D1.1 – 8 inches for welding structural work, in 6G position,

My query is can I use these procedure to weld pipe work as per ASME IX for the same material?

Pls I need further clarification with codes support.

 

Regards

Philip Taiye

 

 
*** WORLEYPARSONS GROUP NOTICE *** "This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it. If you have received this email in error, please notify us immediately by return email and delete the email and any attachments. Any personal views or opinions expressed by the writer may not necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.