Tuesday, September 28, 2010

Re: [MW:7246] MATERIAL TEST CERTIFICATES

Dear Andrews,
 
Katik sir explained it very well. It is totally based on end user requirement.If material details not available in the AFC/IFC drawing review your client specification for structural steel. However, materials with MTC will defenitely give better look for final QC dossier and during Quality Audit on QA/QC documents.
 
 
Regards,
 
Limesh

On Tue, Sep 28, 2010 at 6:41 AM, James cyrilandrew <jcyrilandrew@gmail.com> wrote:

Dear all,
             The thing i have doubt is, for all carbon and alloy steel materials like angles,rod, coil plates,fasteners we can have proper test certificate? because i could not found a correct test certificates for the above said materials. if any one can justify please..... Thank you all. 
--
Regards,
J.C.Andrews
QA/QC Engineer
Doha-Qatar.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...