Hai asad
 
yes u r right at the test limit u have to use temporary gasket. if u use spiralwound it should be replaced with new one to close the re-instatement. it is allowed to use temporary gasket.
THX & RGDS
M.M.REDDY
QA/QC INSPECTOR (WELDING / PIPING)
GAS TO LIQUID PROJECT
ESCRAVOS - NIGERIA
+2347054163177


On Sat, Sep 25, 2010 at 7:16 AM, asad azmi <azmiasadayub@gmail.com> wrote:
Dear All,
 
Please inform me whether  temporary gaskets can be used during hydrotest for process piping at the joint which is a test limit joint where blind/spectacle blind is used.( Construction code B31.3)
 
Example : as per drawing a  particular joint rquires use of 300 #  spiral wound grafite filled SS Gasket. this joint  is the end limit for the particular section.
 
During hydrotest the above joint will be closed/isolated by use of temporary blind flange. so is it allowed to use temporary  gasket such as CAF   at this location.
 
 
Please  give your  comments with respect to code reference.
 
Thanks in advance.
 
Regards
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...