Hi,
All materials have standard specification but Mostly for non pressure parts doesnt require certificates by the customer.When we receive the such materials just refer with the drawing specification and the actual.If you/Customer need the certificates then you should request your supplier to provide the certificates as per the specification you have ordered.
After you receive the certificatesYou can refer with the material specification and according to that you go for the particular standard.
For example,Angle/coil plates - SS400 ....you can refer with JIS standard
Fasteners - A/SA193/194.... - refer to ASTM/ASME
 
Thanks & Regards,
 
(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Tue, 9/28/10, James cyrilandrew <jcyrilandrew@gmail.com> wrote:

From: James cyrilandrew <jcyrilandrew@gmail.com>
Subject: [MW:7230] MATERIAL TEST CERTIFICATES
To: "Material welding groups" <materials-welding@googlegroups.com>
Date: Tuesday, September 28, 2010, 9:41 AM


Dear all,
             The thing i have doubt is, for all carbon and alloy steel materials like angles,rod, coil plates,fasteners we can have proper test certificate? because i could not found a correct test certificates for the above said materials. if any one can justify please..... Thank you all. 
--
Regards,
J.C.Andrews
QA/QC Engineer
Doha-Qatar.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...