Dear Azad..
 
Baking & drying is required for the basic electrodes like E 7018 to reduce the hydrogen content in the deposited weld metal. If you are not doing any baking there by you are improving the condition for hydrogen cracking the weld metal.
 
You have mentioned that you are using E 7018 for the angle bar welding .. normally for structural purpose you can proceed with rutile electrodes like  E 6013 which needs to be dried only.
 
best regards,
 
M.S.Muthu selvam.

On Sun, Sep 26, 2010 at 9:38 AM, asad azmi <azmiasadayub@gmail.com> wrote:
Dear All,
 
Goodday.
 
 
what will be the effect in Mechanical/chemical proerties of deposited weld metal of  E7018 which is used for Structural welding of angle bar( material CS) without drying  (at 260-430deg C) and Holinding(at 120 deg C).
 
 
Can E7018 be used without proper drying and holding for stuructural welding( fillet weld only) of angle bar/supports(material CS).
 
 
Thanks in advance for your valuable suggestions.
 
Best  Regards
 
Asad Azmi
 
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...