Sunday, September 26, 2010

Re: [MW:7201] Hardness of 410

Harish,
 
Are you talking about SA 240 TP 410? Because TP 410 is hardnenable straight-Chromium grade stainless steel .i.e Martensitic stainless steel (P.No. 6). As per specification, the hardness shall be 217 HB max.
 
Anealing this alloy at 1500°F-1550°F (815-842°C) and soaking for one hour per inch of thickness and furnace cool to room temperature may produce a Brinell hardness of 150-192.
Refer this site it may be helpful http://www.sandmeyersteel.com/410.html
 
But TP 410S is non-hardnenable straight-Chromium grade stainless steel .i.e ferritic stainless steel (P.No. 7). As per specification, the hardness shall be 183HB max. The only difference between TP 410 and TP 410S is carbon content and nickel content.
 

 
On Sat, Sep 25, 2010 at 7:23 PM, Harish Kannepalli <harishkannepalli@gmail.com> wrote:
Dear Experts,
                     Can anybody guide me about decreasing the hardness of 410 material from 230HB to 190HB after machining, by heat treatment?

regards,
Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...