               I want to do welding of Hardox 400 Plate to Hardox 400 PLate ,Thickness of both the plate is 40mm. What Type Electrodes I can use?
 
Please suggest me.
 
Regards

Kamaleshwar Kumar Sahu
AGM(QA&I)
Cell: +91 97520 99054