Re: [MW:5309] DP test Requirement in Overlay PQR.

Dear Mr. Rao

As per ASME sec viii div 1,No 42 , VIII-1-98-09,NDT can be performed
before PWHT as well.

in my opinion, Doing a DP test is not a big deal,if client asking for
it,you should fulfill his requirements.

Regards
Manpreet Singh
Welding Engineer
Spiecapag
On Sun, 30 May 2010 12:34:57 +0530 wrote
>
>

>
Dear All,
>

>
I have conducted Overlay PQR qulification (316L OVERLAY ON SA516 Gr.70N) as per ASME Sec IX.
>

>
As per ASME SEC IX QW-453, note 4, 5, 9, we have conducted
>

>
1. DP test after every layer(total 3layers) in as-welded condition.
>
2. 4-Side bend tests in PWHT condition.
>
3. Chemical analysis from overlay specimen in as-welded condition.
>

>
Job requirement:
>
316L weld overlay on SA516 Gr.70, vessel will under PWHT at 620 Deg.C.
>
ASME Div.1 Cladded Vessel.
>

>
Client Comments on PQR.
>

>
client is demanding us to provide DP report After PWHT of the overlay.
>

>
Client says PWHT is essential variable, DP test & bend tests should be conducted after PWHT.
>

>
Query.
>

>
Is it Code (Sec.IX or Div.1 ) requirement to conduct DP test after PWHT ?.
>

>
If it is code requirement, pl. provide the reference from code.
>

>
if any code interpretations available, pl. provide the same.
>

>
regards
>

>
P.Rao.
>

>

>

>

>

>

>

>

>

>

>

>





--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...