Please see the attached file for the IQI details.
Please refer the table in attached file for the relation between different code set and wire number.
Please fill free to contact if any more details required.
Regards, Bhaskar kale
On Sun, May 30, 2010 at 9:55 PM, AGUSTIN JIMENEZ <agumarca@yahoo.com> wrote:
Hi Srinivas.
You can revised in ASME Section 5 Article 2 / T-233 Image Quality Indicator (IQI) Design, API 1104 / 11.1.5 Selection of Image Quality Indicators (IQI), ASTM E 747 or ISO 1027 too.
I hope that it information was utility.Best regards.Agustin Jimenez
De: Srinivas Engr <srinivas.gmsrini@gmail.com>
Para: Materials & Welding <materials-welding@googlegroups.com>
Enviado: dom, mayo 30, 2010 2:20:00 AM
Asunto: [MW:5292] DIN Wire IQI Thickness
Dear All
Where to we find DIN wire IQI Thickness?
Which standard is deals about DIN wire IQI Thickness?
Where to refer?
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
ą¤§ą¤Øą„ą¤Æą¤µą¤¾ą¤¦,
ą¤ą¤¾ą¤øą„ą¤ą¤° ą¤®ą¤Øą„ą¤¹ą¤° ą¤ą¤¾ą¤³ą„
+60149129098
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments