Wire IQI
Used to assess sensitivity ; quality of technique
Pl refer DIN 54109 (1962); ISO 1027 Wire set 1-7; set 6-12; set 10-16 (1,7,6,12,10,16 represent wire numbers)
3 sets - each set having 7 wires (overlapping with adj set) arranged in GP
usually 2% or lesser value of sensitivity is required for general applications
Smaller no 1% indicates higher sensitivity -critical applications
wire dia wire No
mm
3.2 ............... 1
3.2 ............... 1
2.5 ............... 2
2.0 ............... 3
1.6 ...............4
1.25 ...............5
1.0 ...............6
0.8 ...............7
---------------------------
1.0 ..............6
0.8 ...............7
0.63 ...............8
0.50................9
0.40..............10
0.32..............11
0.25...............12
-----------------------------
0.40..............10
0.32..............11
0.25..............12
0.20 .............13
0.15 .............14
0.125............15
0.10 .............16
---------------------------
Regds
MSR
--------------------------------------------------------------------------------------
On Sun, May 30, 2010 at 12:20 PM, Srinivas Engr <srinivas.gmsrini@gmail.com> wrote:
Dear All
Where to we find DIN wire IQI Thickness?
Which standard is deals about DIN wire IQI Thickness?
Where to refer?
--------------------------------------------------------------------------------------------------------------------------------------
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.