Thursday, May 27, 2010

Re: [MW:5276] Tack welder test

Hi
 
You need to qualify the tack welder in each position as per AWS D1.1,
 
You need to weld the test piece as per fig 4.39 of AWS D1.1 (2008 Ed.)


 
On Thu, May 27, 2010 at 8:33 PM, Gulam kader <armvasi@gmail.com> wrote:
Hi to all,

Please explain how to qualify the welder only for tack weld  with code reference.

Regards,

GKM

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Thanks & regards,

K.Babu
Singapore

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...