RE: [MW:5273] Tack welder test

You can qualify them with fillet weld test piece, like 1F, 2F etc.

-----Original Message-----
From: Gulam kader
Sent: 27/05/2010 6:03:21 pm
Subject: [MW:5270] Tack welder test

Hi to all,

Please explain how to qualify the welder only for tack weld with code