Dear Ali,
for your point no. 1, I would like to say due to quenching in oil/water after heating the object to the required temp, the cooling rate will be very faster, so grain size will be less. In this case hardness and brittleness also increases, so to get toughness in the material we need to carry out tempering.

With Regards,
Rutvik
Sr.Surveyor
TATA Projects Ltd.

--- On Wed, 26/5/10, Ali Asghari <asghariali@rocketmail.com> wrote:

From: Ali Asghari <asghariali@rocketmail.com>
Subject: [MW:5257] gorup of SA517
To: materials-welding@googlegroups.com
Date: Wednesday, 26 May, 2010, 4:32 PM

Dear All
1-is Quenching & Tempering a process of grain refining?
2-SA 517 belong to curve A or B in UCS 66?
REGARDS
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...