RE: [MW:5260] Thickness for impact testing

B31.3 thicknesses applicable for PTC and ASME for PQR. Both shall be satisfied.

-----Original Message-----
From: manpreet
Sent: 26/05/2010 12:01:46 pm
Subject: [MW:5253] Thickness for impact testing

Dear All

My case is

Material- Low carbon steel
Applicable code: ASME B 31.3

According to ASME IX QW-403.6, the minimum base metal thickness qulified is the thickness of test coupon T or 0.625" (5/8"), whichever is less. That is 0.5". Therefore, the thickness range 0.25"-0.5" is not qualified.

But the vendor pointed out the the qualified thickness range can based on fabrication code B31.3 Table 323.3.1 which indicates that qualifed thickness range is T/2 to T+0.25".

In this case, what is the minimum qulified thickness: 0.25" or 0.5"? Please advise.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...