Dear Mampreet
My concerns are 2, 1: If I have to do it though my material is ferritic, ASTM A516 grade 70. 2: If I can force the contractor based on the code ??
Thanks a lot
Luis

--- El vie 21-may-10, manpreet <manpreetsin88@rediffmail.com> escribió:

De: manpreet <manpreetsin88@rediffmail.com>
Asunto: Re: [MW:5212] NDT after PWHT
A: materials-welding@googlegroups.com
Fecha: viernes, 21 de mayo de 2010, 6:17


Dear Luis

Currently I am working on LPG Pipeline project.

We have All P1 material, Even then Cpy spec ask for
NDT after PWHT.

When in doubt always go for stringent reference.
Acc to me it's better to go for NDT after PWHT.

Regards
Manpreet Singh
Spiecapag
Welding Engineer
On Thu, 20 May 2010 22:05:58 +0530 wrote
>
Dear friends
We just finished PWHT in an LPG sphere acording to ASME VIII section I, and I can´t find in the code the part that obligues to Xray after this treatment, any one has experience with this? where does ASME VIII say it has to be done?
Thank you
Luis Albanés








--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...