Dear Rao,
No doubts about the client requirement,b'coz always NDT can done after
PWHT.


Thanks,


Sandeep.k.p

On May 29, 2:12 pm, "PAMULA " <vasantharao2...@rediffmail.com> wrote:
> Dear All,
>
> I have conducted Overlay PQR qulification (316L OVERLAY ON SA516 Gr.70N) as per ASME Sec IX.
>
> As per ASME SEC IX QW-453, note 4, 5, 9, we have conducted
>
> 1. DP test after every layer(total 3layers) in as-welded condition.
> 2. 4-Side bend tests in PWHT condition.  
> 3. Chemical analysis from overlay specimen in as-welded condition.
>
> Job requirement:
> 316L weld overlay on SA516 Gr.70, vessel will under PWHT at 620 Deg.C.
> ASME Div.1 Cladded Vessel.
>
> Client Comments on PQR.
>
> client is demanding us to provide DP report After PWHT of the overlay.
>
> Client says PWHT is essential variable,  DP test & bend tests should be conducted after PWHT.
>
> Query.
>
> Is it Code (Sec.IX or Div.1 ) requirement to conduct DP test after PWHT ?.
>
> If it is code requirement, pl. provide the reference from code.
>
> if any code interpretations available, pl. provide the same.
>
> regards
>
> P.Rao.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...