Tuesday, May 25, 2010

[MW:5239] Use of MIG filler wire as a TIG welding filler wire

Dear friends,


i am going to use below ER316LMn filler wire for SS316L. (working condition 4.5K ( -269 'C ) temp.)

ER316LMn filler wire available for TIG & MIG welding. i want to use 1.2 mm dia. filler wire for TIG welding but 1.2 mm dia. not available for TIG welding. 

as 1.2 mm dia. filler available in MIG welding. filler wire mfg. given property for ER316LMn listed below for GTAW & GMAW.

if i want to use MIG filler wire for TIG welding , can I get TIG welding property listed below.

Please give your valuable suggestions.  


Mechanical properties, typical, all weld metal for filler wire ER316LMn

                            Process              Shielding              Condition             0.2% Proof strength              Tensile strength                Elongation               Impact ISO-V(J)
                                                         gas                                                (N/mm2)                                (N/mm2)                          (%)                        -196°C

Typical values          GTAW                  I1                       AW                        430                                        650                               35                              75
                              GMAW                 M12                    AW                        400                                        600                               30                             50



Thanks & Regards,

Hitesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...