I have a already qualified WPS, using which i wanted to qualify few more welders with some variation in material and section used.
 
The following are the WPS parameters: 
Material: A53 Gr B SCH 40 (pipe)
Outer dia: 33.56 mm 1/4" pipe.
Thickness:3.56 mm
Code used for qualification BS 15609 & 15614.
Welder qualification carried out as per BS 287-1.
 
How can i qualify the welders with RHS(rectangular Hollow section)with max thickness of 12 mm & SHS (square hollow section)
also i wanted to use ASTM A500 grade C(tube).
 
1.Please explain whether i can qualify the welders using the same WPS with some alterations.
 or a entirely new WPS to be written.


--
Thanks and Regards

Nishad AK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...