[MW:4542] Re: Welding of Brasses & Bronzes

Hi Prem
Many thanks for your reply. I have already consulted these documents.
But there is only a standard composition against each electrode coding
but unfortunately there is no selection criteria of electrodes for
Brasses,Bronzes and Cast Iron. For example in some applications we use
an electrode that gives the deposit of 60% Ni and rest of Fe for Cast
Iron Welding where as sometimes we use the electrode that gives 55% Ni
for the same kind of applications and sometimes we use an electrode
that gives 99.99% Ni. But I dont know the selection criteria. I mean
why dont we use an electrode that gives exactly the Cast Iron
composition. Same is the case with Brasses and Bronzes. I hope that I
have explained my problem.

On Mar 9, 10:15 am, "PREM SHANKARDUTT NAUTIYAL"
<prem_nauti...@rediffmail.com> wrote:
> Hi Uzzmaan
>
> You better read the following specifications in ASME Sec II Part C :
> 1) SFA 5.6 - Covered copper and copper alloy arc welding electrodes, 2) SFA:5.7 - Copper and Copper Alloy bare welding rods /electrodes, 3) SFA 5.15- Welding electrodes and rods for Cast iron.
>
> You will get your answers.
>
> If you still have any doubts then post your queries which will be answered immediately..
>
> Regards
>
> Prem Nautiyal
> Mumbai.
> Cell: 9820313278
>
> On Tue, 09 Mar 2010 08:45:26 +0530  wrote
>
> >Hey Guys how r u?
>
> I m Uzzmaan and I hv recently joined this group. Can any body tell me
>
> that what is the criteria to select the SMAW electrode to join cast
>
> Iron, Brasses & Bronzes? I mean what is the criteria to select the
>
> electrode that will join Brass or that can be used to fill the
>
> porosities present in the cast iron,brass or bronze castings?
>
> --
>
> To post to this group, send email to materials-welding@googlegroups.com
>
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
> For more options, visit this group's bolg athttp://materials-welding.blogspot.com/
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
> PREM S NAUTIYAL
> CELL : 9820313278

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...