RE: [MW:4609] RE: 4606] RE: 4605] Welding consumable for SS 329

THE MATERIAL NO. IS 1.4460 WITH DIN DESIGNATION X 3 CrNiMoN 27 5 2.
 
THE ELECTRODE MAY BE USE 6810 MoKb and TIG RODS / MIG WIRES A6810Mo
 
THIS IS WITH REFERENCE TO UTP WELDING CONSUMABLES
 
AWS EN TESS Engros  Esab Elga Böhler Thyssen Soudokay UTP AWS EN AVESTA Metrode Selectarc Lincoln
A5.4/A5.11 EN1600   OK Cromarod FOX Thermanit     A5.4/A5.11 EN1600        
2209-15 22 9 3 N L B 2205 Bas 67.55 Duplex B CN 22/9 N-B 22/09 SOUDINOX S 4462 6808 MoKb 2209-15 22 9 3 N L B 2205 Bas 2205XKS Inox 2209 B Jungo Ziron 100 X

 
 
 
regards,
 
Farhan Talib


 
 



 
> From: mehmood.javed@fatima-group.com
> To: materials-welding@googlegroups.com
> Subject: [MW:4608] RE: 4606] RE: 4605] Welding consumable for SS 329
> Date: Thu, 25 Mar 2010 16:08:41 +0500
>
> UNS # is S32900
>
> Regards,
>
> Mahmood
>
> -----Original Message-----
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Raghuram
> (Mumbai - PIPING)
> Sent: Thursday, March 25, 2010 1:18 PM
> To: materials-welding@googlegroups.com
> Subject: [MW:4606] RE: 4605] Welding consumable for SS 329
>
> Pl specify UNS# or full specification, if it is for UNS# S32950/F52, you
> may use E/ER 2209
>
> -----Original Message-----
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of Mehmood Javed
> Sent: Thursday, March 25, 2010 11:56 AM
> To: materials-welding@googlegroups.com
> Subject: [MW:4605] Welding consumable for SS 329
>
>
> Dear All,
>
> Can somebody let me know the welding consumable specifications for SS
> 329 forging,
>
> Regards,
>
> Mahmood
>
>
>
> Filtered by Hosted Filtering
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
> To unsubscribe from this group, send email to
> materials-welding+unsubscribegooglegroups.com or reply to this email with
> the words "REMOVE ME" as the subject.
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
> To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.


Hotmail: Trusted email with Microsoft's powerful SPAM protection. Sign up now.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...