Skip to main content

Re: Re: [MW:4561] Tracer Joints

Hi friend,
If the 32 welds were made by a single welder, in this case should select 2 weld, and if your rejections are 8 joints.
You should evaluate all joints.

Kind regards.
Gustavo Mendoza.
QA/QC Inspector.
Venezuela.


mar 13, 2010 03:50:32 AM, materials-welding@googlegroups.com wrote:

===========================================

Good day. The problem we are facing from our contractor are as under: We got the Radiography result of our process piping joint with very poor quality. Radiography performed @ 5%. Totao RT Joints= 32, Repair= 12, Cut-out=02, so kindly advise can we extend the Radiography percentage as well as Tracer or pnalty joints??? PLEASE ADVISE   
 
Regards

 
Syed Arshad Farooq 
 QA / QC Engineer

 PROCTER & GAMBLE
 D.L UNIT KARACHI
(+92-21-111-284-284,5378637-40
): +92-308-3067599


From: "agmendoza@cantv.net"
To: materials-welding@googlegroups.com
Sent: Fri, March 12, 2010 10:13:26 PM
Subject: Re: [MW:4546] Tracer Joints


Hi, friend
ASME B31.3, do not state anythig about repair twice time on same joint.
Regarding repairs the code state:

341.3.3 Defective Components and Workmanship.
An examined item with one or more defects (imperfections of a type or magnitude exceeding the acceptance criteria of this Code) shall be repaired or replaced; and the new work shall be reexamined by the same methods, to the same extent, and by the same acceptance criteria as required for the original work.

341.3.4 Progressive Sampling for Examination.
When required spot or random examination reveals a defect, then (a) two additional samples of the same kind (if welded or bonded joints, by the same welder, bonder or operator) shall be given the same type of examination
(b) if the items examined as required by (a) above are acceptable, the defective item shall be repaired or replaced and reexamined as specified in para. 341.3.3, and all items represented by these two additional samples shall be accepted, but (c) if any of the items examined as required by (a) above reveals a defect, two further samples of the same kind shall be examined for each defective item found by that sampling (d) if all the items examined as required by (c) above are acceptable, the defective item(s) shall be repaired or replaced and reexamined as specified in para. 341.3.3, and all items represented by the additional sampling shall be accepted, but (e) if any of the items examined as required by (c) above reveals a defect, all items represented by the progressive sampling shall be either
(1) repaired or replaced and reexamined as required, or
(2) fully examined and repaired or replaced as necessary, and reexamined as necessary to meet the requirements of this Code
(f ) If any of the defective items are repaired or replaced, reexamined, and a defect is again detected in the repaired or replaced item, continued progressive sampling in accordance with (a), (c), and (e) is not required based on the defects found in the repair. The defective item(s) shall be repaired or replaced and reexamined until acceptance as specified in para. 341.3.3. Spot or random examination (whichever is applicable) is then performed on the remaining unexamined joints.

I understand the above paragraphs is that the joint should repair again but without tracer.

Kind regards.

Gustavo Mendoza.
QA/QC Inspector.
Venezuela.

mar 12, 2010 03:55:14 AM, materials-welding@googlegroups.com wrote:

===========================================

According to ASME B31.3 ,after NDT if repair twice time on same
joint,what will be procedure as per ASME B 31.3 for tracer joint /
Panely joint

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

     

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...