Re: [MW:4532] Hardness value of A543 Type-B, Class-1

i could able to locate some info on this material, pl refer the attachement on file section of the group titled environmental stress cracking.http://groups.google.co.in/group/materials-welding/files

Hardness diff stated in ASME is applicable only for forged vessels, however in case div3 vessels it may be applicable for welded ones also.
Since Hardness is not given in the code for this material, and PWHT not mandatory either, what is your contract says?

check the original material hardness, and compare it with the weld metal, what difference you are getting? Plate mill may be in better position to help, check with mills like dillinger.

this is similar to HY 80 materail
 
On Tue, Mar 9, 2010 at 10:42 PM, juttada venugopal <jamsvenu@gmail.com> wrote:
Dear All,
 
  1. May I please know the hardness values of quenched and tempered steel of material A543, type-B, class-1.at the locations of parent metal, weld and HAZ 
  2. What shall be the variation in hardness allowed for this material prior to and after post weld heat treatment. As per Secion 8 div's, variation (min to max.) in hardness of 40 is permitted, is it the same for this material also or any exceptions.
Please share your views, any feed back is appreciable. 
 
Thanks and regards,
 
Venugopal
==========================
. 
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...