Re: [MW:4142] Is PCN L-III is qualified to certify ASNT L-II ?

Greeting All,

In addition to the well address response from Mr. Ragvendran,

Any ASNT NDT Level-III qualified and certified technician in NDT Level-I and II only as per the employer written practice.

To get the LEVEL-III qualified as per the employer written practice, written practice shall address the qualification and certification procedure for Level-III.

If the employer mention in the procedure PCN Level-III is appointed directly as his Level-III then he can qualified and certified the NDT level-I and II tech for the employer and certificate will issue as per the procedure only as NDT level I and II and not as "ASNT NDT LEVEL-I OR II ".

Most important governing document is employers written practices.

Regards,

Bhaskar Kale



On Sat, Jan 23, 2010 at 10:59 AM, PEMMARAJU RAGHAVENDRA <rpe@hzw.ltindia.com> wrote:
Dear Mr.Vasanth,
Pl.note that there is no ASNT Level II. ASNT issues only ASNT NDT Level III and ACCP Level IIs.
An ASNT NDT Level III / ACCP L-III can issue L-I or II certificates as per SNT-TC-1A.
Any organisation who intend to have an NDT deptt. shall have their own NDT personnel Qualification Written Practice which is based on SNT-TC-1A.
In that written practice,if the employer mentions that even a PCN Level III qualified person can certify their NDT personnel as L-I or II, the same is acceptable.
Hence, in your case, pl.have your own Written practice for training, qualification and Certification of NDT personnel in which you can mention PCN L-III can issue L-II certificates.

In short, as per the reference doc.SNT-TC-1A, have your Written practice to incorporate your requirement.

Regards,
Raghavendra

Larsen & Toubro Limited
www.larsentoubro.com

This Email may contain confidential or privileged information for the intended recipient (s) If you are not the intended recipient, please do not use or disseminate the information, notify the sender and delete it from your system.


>>> "Chandra, Vasanthan (Lagos)" <Vasanthan.Chandra@DeltaAfrik.com> 22/01/2010 10:00 pm >>>
Friends,



Can any one Pl confirm that PCN L-III is qualified to certify ASNT L-II?
If yes, Pl provide me reference document.



Regards,
Vasanth





*** WORLEYPARSONS GROUP NOTICE ***
"This email is confidential.  If you are not the intended recipient, you must not disclose  or  use the  information contained in it.
If you have received this email in error,  please notify us immediately by return email and delete the email and any attachments.
Any personal views or opinions expressed by the writer may not
necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
धन्यवाद,
भास्कर मनोहर काळे

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...