Monday, September 14, 2009

[MW:3188] Re: Ferrite limits

3 (minimum) to 7 % (max) or 4 ( min) to 6% (max) depending on the
application ( Nuclear Reactors applications)
Regards,
Vaidehi Ganesan.
--------------------------------------------------------------------------------------------------------------------------------
----- Original Message -----
From: "ma" <azizi-m@pidec.com>
To: "Materials & Welding" <materials-welding@googlegroups.com>
Sent: Sun, Sep 13, 09 5:28
Subject: [MW:3185] Ferrite limits


>
> Hi every body
> what is the acceptable criteria of Ferrite phase during the Stainless
> Steel weding?
>
> Thanks
> MA
>
>

--------------------------------------------------------------------------------

No virus found in this incoming message.
Checked by AVG - www.avg.com
Version: 8.5.409 / Virus Database: 270.13.95/2368 - Release Date: 09/13/09
17:50:00


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...