[MW:3187] Re: Ferrite limits

According to API 582 (6.3)   3-11 FN ( austenatic SS except 347 min is FN 5)  ,
generally client makes it  3 to 8 ( Shell DEP or PTS )
For detalis requirement refer API 582 or Client's tech. spec.
 
regards,

On Sun, Sep 13, 2009 at 7:58 PM, ma <azizi-m@pidec.com> wrote:

Hi every body
what is the acceptable criteria of Ferrite phase during the Stainless
Steel weding?

Thanks
MA


--
Sukamal


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...