[MW:3186] Re: Welding Issue

ASME Sec-IX 2007 ed 2009 add, has removed the S-No. , now all are P No. hence API 5L  gr. X52  is P no.1 Gr. no.1 material.
 
regards,

On Thu, Sep 10, 2009 at 8:44 AM, Juan Coello <jacoello87@gmail.com> wrote:

Hello, I'm in need of your knowledge, I need to make a WPS and a PQR
to weld  two materials, both are api 5lx52 schedule 120 outside
diameter16", I cannot determine nor find the P number nor Group number
of this material.

I am also trying to determine what types of electrodes to use, wether
E60XX or E70XX if I'm not mistaken nor how many passes to make (I'm
thinking abot 6).

Thank you and hoping for a response





--
Sukamal


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...