Tuesday, February 10, 2009

[MW:1537] Re: minimum length

Dear Mr. Nilesh,

 

Could you pls give the reference paragraph in the ASME B 31.3 which mentions this?

 

I heard it shall be 5t or min 300mm for the size of a pup piece. No where in the ASME B 31.3 I could see it mentioned. Correct me if I'm wrong.

 

Thank you,

 

Regards,

 

 

Sabir 



On Tue, Feb 10, 2009 at 11:28 AM, nilesh <nilesh_parsekar@yahoo.com> wrote:
Dear Javed,
 
   As per ASME 31.3 it should be 150mm

 Nilesh Parsekar,
 QC CO-ORDINATOR
(Dp Mech,API 510,API 570,AWS-CWI,NDT LEVEL2)
 Belleli Energy
 QATAR


--- On Tue, 2/10/09, Mohammad Javeed <mmubasharjaveed@gmail.com> wrote:
From: Mohammad Javeed <mmubasharjaveed@gmail.com>
Subject: [MW:1534] minimum length
To: materials-welding@googlegroups.com
Date: Tuesday, February 10, 2009, 1:09 AM


dear all, have a nice day
can any one tell me what is a  minimum length between two butt joints.( piece of pipe) with reference
thanks with regards
m javed





--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...